Our factory have 2 advanced automated coating lines, all performance parameters are up to or much higher than related national standards.
RawMaterial:the alloy of Aluminum AA1100, AA3003, AA5005
Paint:Polyester or PVDF KY
PE Coil is widely and mainly used for building decoration, such as ACP, aluminum ceilings, aluminum sheets, honeycomb panels and aluminum roofing, lighting decoration, household electrical appliance, food package, furniture etc.
Items |
Test Item |
Standard |
National Standard |
Test Report |
1 |
Color Difference |
ECCA T3 |
△E<= 2.0 |
△E<= 1.5 |
2 |
Gloss Difference |
ECCA T2 |
<= 10 |
<= 5 |
3 |
Coating Thickness |
ECCA T1 |
Min 14 Micron |
Min 16 Micron |
4 |
Pencil Hardness |
ASTM D3363 |
>= HB |
>= HB |
5 |
T-Bend |
ASTM D4145 |
<= 3T |
<= 2T |
6 |
Adhesion |
ASTM D3359 |
Grade 0 |
Grade 0 |
7 |
Impact |
ASTM D2794 |
>= 20Kg.cm |
>= 20Kg.cm |
8 |
Boiling Water Resistance |
GB/T 17748 |
2h no change |
2h no change |
9 |
Solvent Resistance |
ASTM D2248 |
200times paint |
200times paint |
10 |
Salt Resistance |
ASTM B117 |
720Hrs<= Grade 1 |
720Hrs<= Grade 1 |
11 |
Dirt Resistance |
GB/T 9780 |
<= 5% |
<= 5% |
12 |
Color Retaining |
GB/T16259 |
600 hrs△E<= 2 |
△E<= 2 |
13 |
Gloss Weaken Level |
600 hrs <= Grade 2 |
<= Grade 2 |
|
14 |
Chalking |
600 hrs no change |
no change |
Items |
Test Item |
Standard |
National Standard |
Test Report |
1 |
Color Difference |
ECCA T3 |
△E<= 2.0 |
△E<= 1.5 |
2 |
Gloss Difference |
ECCA T2 |
<= 10 |
<= 5 |
3 |
Coating Thickness |
ECCA T1 |
Min 14 Micron |
Min 16 Micron |
4 |
Pencil Hardness |
ASTM D3363 |
>= HB |
>= HB |
5 |
T-Bend |
ASTM D4145 |
<= 3T |
<= 2T |
6 |
Adhesion |
ASTM D3359 |
Grade 0 |
Grade 0 |
7 |
Impact |
ASTM D2794 |
>= 20Kg.cm |
>= 50Kg.cm |
8 |
Boiling Water Resistance |
GB/T 17748 |
2h no change |
2h no change |
9 |
Solvent Resistance |
ASTM D2248 |
200times paint |
200times paint |
10 |
Salt Resistance |
ASTM B117 |
720Hrs<= Grade 1 |
720Hrs<= Grade 1 |
11 |
Dirt Resistance |
GB/T 9780 |
<= 5% |
<= 5% |
12 |
Color Retaining |
GB/T16259 |
600 hrs△E<= 2 |
△E<= 2 |
13 |
Gloss Weaken Level |
600 hrs <= Grade 2 |
<= Grade 2 |
|
14 |
Chalking |
600 hrs no change |
no change |